Why a BLE or UWB device resets on a coin cell: pulse current, voltage sag and the buffer capacitor
A coin cell resets a BLE or UWB device when the radio’s current pulse, multiplied by the cell’s internal resistance, pulls the supply below what the chip needs, often while the cell still holds a useful part of its charge, especially on UWB, in the cold or at a low average drain. A CR2032 lithium cell starts near 10 ohms and rises as it discharges and gets cold, so a 30 mA pulse that costs 0.3 V on a fresh cell costs 0.9 V at 30 ohms, where one chip maker’s tests found cells reaching a 2.0 V cutoff. UWB is the harder case: one UWB transceiver draws 48 mA to transmit and 78 mA to receive during a ranging exchange, against about 6 to 9 mA for BLE radios, and its main radio supply needs at least 2.4 V. A buffer capacitor sized from C = I·t/ΔV for the whole burst carries the pulse so the cell only refills it, and a UWB node that listens continuously needs a bigger battery than a coin cell.
The usual report is a product that fails in the field after a few months, or only outdoors in winter, while a multimeter reads the cell as healthy: the meter draws almost nothing, so it sees the voltage behind the resistance. The power budget itself is in Battery-powered design.
A coin cell is a voltage source behind a resistor
A 2032 coin cell is lithium manganese dioxide, nominally 3.0 V, rated by one maker at 225 mAh to 2.0 V through 10 kΩ at 21 °C, about 0.29 mA: nothing like a radio burst.
Lithium coin cells have a much higher internal resistance than other common chemistries: a 2032 starts near 10 ohms, an AA alkaline cell near 0.25 ohms. One maker’s handbook measures it from a pulse: 3.279 V at 3 µA falling to 2.429 V at 97 mA is about 9 ohms, and drain rate and pulse length change the answer. After long storage a cell starts slightly higher, until a load thins its passivation layer.
Resistance rises as the cell discharges, as reaction by-products build up, and the same handbook plots how. Pulsed at about 30 mA for 0.1 s every 5 s, its 2032 stays at about 13 to 16 ohms from 25 to 100 mAh used, reaches about 18 ohms at 150 mAh and about 30 ohms near 185 mAh, then climbs to about 65 ohms as the cell ends, near 210 mAh. Its open-circuit voltage between pulses starts above 3.1 V, drops to around 2.8 V within the first few mAh, sits at about 2.88 V from about 25 to 100 mAh, and reaches about 2.8 V at 150 mAh and about 2.6 V at the end. That’s one maker’s typical cell in a room-temperature test (the figure doesn’t print the temperature), and vendors spread widely, as the next section shows. Through most of the discharge the meter reading barely moves while the resistance that decides the pulse climbs.
The pulse test suits a product that’s busy. A tag that averages microamps follows the handbook’s 3 µA curve instead, which rises much sooner: about 20 ohms at 50 mAh, about 55 at 75 mAh and over 100 ohms by 90 mAh, with a warning that very low drain rates can raise the resistance early in the discharge. Cold raises it too, as a later section covers.
Why the average current says nothing about the pulse
Capacity divided by the average current gives a battery life, but says nothing about the peak. One cell maker puts it plainly: in high-pulse applications the voltage during the pulse meets a 2 V cutoff much sooner than the average drain predicts. Its 30 mA pulse test averages 0.6 mA, but the cell only ever “ends” during a pulse.
So check two things: the average, for how long the cell lasts, and the lowest voltage at the worst moment, with the cell’s end-of-life resistance at the lowest temperature.
A chip maker’s 2010 white paper tested at least twelve cells from each of six vendors on a repeating load of 8 mA for 2 ms, a peak for 1 ms, 8 mA for 2 ms and 0.1 mA for 200 ms, to 2.0 V. Raising the peak from 15 mA to 30 mA cut effective capacity by only 9 percent on average, while some vendors’ cells delivered only about half their rated capacity at either peak.
BLE pulses against UWB pulses
Everything above gets harder with UWB. A UWB receiver draws more than ten times what a BLE radio does, the chip holds a high current through the whole exchange rather than one packet, and its supply floor sits above the voltage the cell’s capacity is rated to.
| Radio (one datasheet each) | Receive | Transmit | Lowest supply |
|---|---|---|---|
| BLE chip | 5.9 mA | 6.1 mA at 0 dBm, 9.1 mA at +5 dBm | 1.8 V |
| Second BLE chip | 6.5 mA | 7.1 mA at 0 dBm | |
| UWB transceiver, ranging exchange | 78 mA (preamble), 70 mA (frame) | 48 mA (preamble), 40 mA (frame) | 2.4 V on the main radio supply |
| UWB transceiver, continuous receive | 72 mA (lower channel), 88 mA (higher channel) | ||
| UWB module, no frames received | 50 mA, 55 mA | 40 mA, 45 mA | 2.5 V |
The rows come from different chips, revisions and supply modes; the UWB transceiver’s 78 mA and 72 mA are both as printed, from different parts of its datasheet.
Most coin-cell advice was written for BLE, and I think it’s the wrong starting point for UWB: the currents are five to thirteen times larger, the supply floor is higher, and the margins that make a BLE design forgiving aren’t there.
A ranging exchange is a sequence of bursts
One UWB transceiver’s datasheet draws the initiator’s side of a double-sided two-way ranging exchange. The chip leaves deep sleep and starts its oscillator, about 1 ms at 1.5 mA, then idles at 8 mA on its internal clock and 18 mA once its synthesizer is locked. It transmits the poll, about 170 µs at 48 mA, waits at 18 mA, receives the response, about 170 µs at 78 mA, waits at 18 mA again, transmits the final message, about 170 µs at 48 mA, and returns to deep sleep at 260 nA.
Each burst is short, but between them the chip sits at 18 mA, twice a BLE radio’s peak. The receiver’s preamble hunt also runs for a variable time at 70 mA, so a receive window opened early for timing margin costs 70 µC per millisecond of margin, more than the whole exchange budget worked out below. The datasheet’s row labelled “Current single frame Tx/Rx with 47uF capacitor”, at 3.0 V supplies, gives 14 to 19 mA depending on channel and direction; that reads as the battery-side current over a frame once the capacitor smooths it, though the datasheet doesn’t define it further.
Supply floors above the cell’s rated cutoff
Cell makers rate capacity to 2.0 V, but the UWB transceiver’s main radio supply needs 2.4 V plus headroom for ripple, and a UWB module’s supply 2.5 V. A UWB part can’t use the capacity below that floor, and the headroom above it is small. State by state on the handbook’s curve, remembering that its resistance came from a 30 mA, 0.1 s pulse, not a 78 mA, 170 µs one:
- A fresh cell, above 3.1 V and about 10 ohms, sags to about 2.3 V on the 78 mA burst, already below the floor.
- At mid-life, about 2.88 V and 13 to 16 ohms, it sags to about 1.6 to 1.9 V. Carrying the burst directly there would take about 6 ohms.
On a UWB tag, then, the buffer capacitor is what makes the design work at all. Feeding one of the transceiver’s rails from an efficient switching regulator at 1.6 V cuts its peak currents significantly, but leaves the 2.4 V floor on the main radio supply where it is. And on a product with both radios, a module maker warns that a UWB current spike landing while the host or BLE radio is busy could brown out or reset the UWB chip, so add up everything that can be on at once.
A listening responder is a different case from a tag
That’s the tag’s side. The responder has to be listening when the poll arrives, and the same module maker is direct: responders listen continuously, that receive current is too high for a battery, and tags, which don’t need to listen, can run on one. A module listening at 50 mA would empty a 225 mAh cell in 4.5 hours, drawing about seventeen times one older sheet’s 3.0 mA maximum continuous current. A fresh cell would hold about 2.6 V at first, just above the module’s 2.5 V floor, but the load is continuous, not a pulse. A node that listens needs mains power or a much larger battery, and this article doesn’t size that side.
What the chip does when the supply dips
A brownout reset holds a chip in reset while its supply is below a threshold. Two low-power radio chips’ datasheets put the falling threshold at 1.67 V on one and typically 1.65 V on the other, with 10 to 20 mV of hysteresis: below the 2.0 V the cell is rated to, and on the first chip just below its own 1.71 V operating minimum, so the brownout isn’t the line to design to. A third chip offers a power-fail comparator, programmable from 1.7 V to 2.8 V, that warns the processor without resetting it.
For a BLE-only design those numbers are forgiving. Near the end of the handbook’s test, at about 2.6 V and 65 ohms, a BLE chip that runs down to 1.8 V can still take about 11 mA from the cell with a 0.1 V margin, which covers its radio’s peak. On a UWB tag the binding limit is the transceiver’s 2.4 V minimum, where operation is guaranteed only within the supply ranges. If its radio supply dips to 2.3 V while the processor carries on above its brownout, nothing resets and nothing is guaranteed. Design to the highest minimum supply of anything on the rail, measured at the chip’s pin.
When a dip does reach the reset threshold, the result is often a loop: the chip resets, its load falls, the cell recovers through its resistance by far more than a 10 to 20 mV hysteresis band, the chip boots, starts the radio and pulls the supply down again. The product looks dead with a cell that still holds charge. What breaks the loop is a firmware check of the cell before the first heavy burst, or a supervisor whose release threshold sits deliberately above its reset threshold. A reading taken during a burst shows what the cell can deliver, so a product nearing the floor can range less often instead of resetting; the article on battery percentage covers reading a cell under load.
The peak-current limits that disagree
Published peak-current figures for coin cells disagree because they answer different questions. One maker’s 2032 sheet prints a maximum pulse current of 15 mA, and its 1,000 mAh 2477 sheet 25 mA, without saying for how long or to what cutoff. Others give only test conditions, such as a 400 ohm pulse for 2 seconds, about 6.8 mA.
A 15 mA figure also circulates as a hard limit, which the 2010 white paper was written to answer: 30 mA cost only about 9 percent of capacity, and 15 mA wasn’t enough to get good capacity from every vendor’s cells. Another chip maker’s 2026 coin-cell note proposes keeping the peak below 10 mA, “as recommended by coin cell manufacturers”, a figure it attributes to the cell makers rather than measures, and meets with series resistors and a 47 µF input capacitor, holding the peak to 8 mA.
The white paper’s measured resistance limit was about 30 ohms for a 30 mA peak and about 60 ohms for a 15 mA peak. Both products come to 0.9 V, about the headroom between a mid-life cell’s 2.88 V and a 2.0 V cutoff. So the limit is a voltage drop, not a current: the peak drawn from the cell, times its resistance at end of life and lowest temperature, has to stay below its open-circuit voltage minus the highest minimum supply on the rail, less a margin for ripple.
For a UWB tag with a 2.4 V floor and the 0.1 V margin used below, that allows about 17 mA from the cell at 150 mAh used (about 2.8 V and 18 ohms) and about 1.5 mA at the end of the pulse test (about 2.6 V and 65 ohms). On the 3 µA curve, at about 100 ohms by 90 mAh, it’s about 4 mA. Somewhere along the way the tag stops working while the cell still has charge a BLE device could use.
Sizing the buffer capacitor
A capacitor across the supply carries the burst, its voltage falling by the charge drawn divided by its capacitance. So C = I·t / ΔV, summed over the burst, where ΔV is the starting voltage minus the lowest the rail may reach; as the white paper puts it, the total charge matters, not the peak. Its fuller formula credits the charge the cell supplies during the burst, a credit that shrinks as the resistance rises, so the plain formula is the end-of-life case.
A BLE event
The white paper’s own load, 8 mA for 2 ms, 30 mA for 1 ms, 8 mA for 2 ms, draws 62 µC. Allowing a fall from 2.6 V to 2.0 V, the plain formula gives about 103 µF; the paper credits the cell with 2 mA over the 5 ms, assuming 1 kΩ of source resistance, and gets 87 µF. Adding a capacitor improved the worst cell by more than 40 percent.
On a chip maker’s support forum, a BLE device sending three advertisements of about 10 mA for 380 µs each, by the poster’s estimate, failed in a freezer at about −10 °C with 4.7 µF and worked with 47 µF. Back to back, that’s about 11.4 µC, a 0.24 V drop from 47 µF but 2.4 V from 4.7 µF, so the cold cell had to carry it and couldn’t.
A UWB ranging exchange
The initiator’s three bursts, 48, 78 and 48 mA for about 170 µs each, draw 29.6 µC. The chip idles at 18 mA between them for as long as the reply delays the firmware sets; take 1 ms in total as an example, which adds 18 µC, for about 47.6 µC. Treat that as a floor: it leaves out the idle before the poll (8 mA, then 18 mA while the synthesizer locks), the host’s own activity on the bus, and any preamble-hunt margin.
Start from the mid-life 2.88 V and stop at the 2.4 V floor plus 0.1 V for ripple (an example margin): ΔV is about 0.4 V, and the capacitor needs at least about 120 µF of real capacitance at its working voltage and lowest temperature. At 150 mAh used, from about 2.8 V, it’s about 160 µF, and at the end of the pulse test, from about 2.6 V, ΔV is only 0.1 V and it’s about 480 µF. With a capacitor, then, the limit is the shrinking ΔV as the open-circuit voltage falls toward the floor. The datasheet’s typical 47 µF would fall 0.63 V on the three bursts alone, from 2.88 V to about 2.25 V, unless the cell helps; a fresh cell helps far more than a cold, part-used one. Count retries, longer receive windows, the higher channel and coincident BLE events too.
Real capacitance, ESR and temperature
The formula needs the capacitance the part delivers in the circuit. Ceramics lose capacitance under DC voltage, and one maker’s note adds a further gradual loss of up to 20 percent over up to 1,000 hours, advising designers to oversize in rated voltage or capacitance; another maker rates this bias dependency high for ceramics, medium for solid tantalum and low for aluminium electrolytics and polymer hybrids. No sourced figure gives the loss for a 47 to 100 µF ceramic at 3 V, but it can be large enough that the nominal value has to sit well above 120 µF, so read the maker’s curve for the exact part, or measure it.
Temperature takes more. That second maker’s guide gives the change in capacitance at −40 °C, against 20 °C, as about −10 to −20 percent for aluminium electrolytics, −10 to −15 percent for polymer hybrids and −2 to −4 percent for solid tantalum, with an aluminium electrolytic’s impedance rising steeply in the cold and a hybrid’s much flatter. Its −40 to −60 percent for high-dielectric ceramics matches the high-loss Y5V and Z5U classes; the X5R and X7R parts a buffer like this would use are specified to stay within ±15 percent over their temperature range, on top of the bias loss.
The capacitor’s equivalent series resistance (ESR) adds an instant step, I × ESR, at each burst: at 78 mA every ohm costs 78 mV of a 0.4 V budget. So the budget is Q/C plus I × ESR at the lowest operating temperature, with the capacitor close to the radio’s supply pins.
Capacitor leakage against the sleep budget
A capacitor across the cell raises the usable capacity and adds its leakage to the sleep current, here against a transceiver deep sleep of 260 nA.
One engineer measured roughly 70 to 80 nA for both a 200 µF ceramic and a 470 µF aluminium electrolytic. Taking that single measurement as the scale, 80 nA adds about 30 percent to the deep-sleep current and costs about 0.7 mAh a year, small against 225 mAh. Leakage moves, though: an aluminium electrolytic’s rises after long storage, one polymer tantalum series allows up to ten times its initial leakage at 85 °C, as a test limit, and a forum reply warns that tantalum’s high leakage suits it only for short-term storage. Take the leakage at your voltage and highest temperature from the datasheet and give it its own line in the budget.
A supercapacitor is a different order: one 1 F part’s maximum leakage of 6 µA, after 72 hours, is about 53 mAh a year, close to a quarter of the cell.
A series resistor to limit the recharge current
After the UWB exchange, with the capacitor 0.4 V down, a 10 ohm cell starts refilling it at 40 mA: a peak after all, just later. With 10 ohms in line (an example value), the refill starts at 20 mA, and the inrush when a fresh cell goes into a board with an empty capacitor roughly halves, from about 300 mA. The capacitor goes on the load side of the resistor, as in the 10 mA note above.
The cost is refill time, which the white paper gives as t = R·C·ln((Vp − Vmin) ÷ (Vp − Vmax)), with Vp the cell’s unloaded voltage. For the 120 µF example, refilling from 2.5 V to within 50 mV of a 2.9 V cell takes about 5 ms through 20 ohms (cell plus resistor), 10 ms through 40 ohms (a 30 ohm cell plus resistor) and 250 ms through 1 kΩ, longer than the 100 ms between exchanges at a 10 Hz ranging rate. Use the end-of-life resistance in R, against the shortest gap the firmware can produce.
The resistor also limits what the cell can feed the idle current. At 18 mA through 20 ohms the supply settles toward a 0.36 V drop, with a 2.4 ms time constant at 120 µF, nearly the whole 0.4 V budget, and through 40 ohms the settled drop is 0.72 V. A long idle before the first burst eats the budget, so keep it short. The ranging example in the next section averages 0.49 mA, and at that current the 10 ohm resistor drops about 5 mV. Since halving the peak gained only about 9 percent of capacity in the white paper’s tests, the resistor is mainly a way to meet a cell maker’s pulse recommendation and limit inrush.
Cold
Cold slows the reactions inside the cell and reduces ion mobility in its electrolyte, so its resistance rises; once the cell warms up, its voltage and capacity recover, which is why a product that fails outdoors in winter can work again on the bench.
One maker of a wide-temperature 2032 plots resistance at −40 °C, 23 °C and 125 °C on one graph. All three curves start near 10 ohms; after 100 hours the −40 °C curve is at about 38 ohms against about 25 at 23 °C, and after 600 hours about 67 against about 42. The axis is storage time and the sheet doesn’t say what load was applied, so it can’t size a design; read it only as a ratio, with the cold cell at least about one and a half times the resistance at both points read.
No maker publishes resistance against depth of discharge and cold together, so measure it late in the cell’s life at the product’s lowest temperature: it’s the number every calculation above needs. The white paper notes that the capacitor matters even more in the cold, when an aluminium electrolytic has lost some of its capacitance and its impedance has risen.
When a coin cell can’t do it
The capacitor solves the peak, not the energy. The exchange above, start-up included, is about 49 µC. Ranging ten times a second (an example rate) averages about 0.49 mA before sleep current, and a 225 mAh cell lasts at most about 460 hours, roughly 19 days; once a second, at most about 190 days. Both are ceilings: the charge budget is a floor, and they come before losses to the 2.4 V floor, pulses and cold. And 0.49 mA is well above the 0.29 mA standard test drain the capacity is rated at. The battery life estimator runs the energy side with your own numbers.
When the arithmetic doesn’t close, change the cell or the power design.
A larger lithium cell buys capacity and some pulse capability: one maker’s 1,000 mAh 2477 lists a 25 mA maximum pulse against 15 mA for its 2032, without a resistance. A 3.6 V lithium thionyl chloride AA cell is rated for pulses typically up to 250 mA for 0.1 s when undischarged, and its maker notes that pulse readings vary with temperature and the cell’s history; another maker pairs that chemistry with a hybrid layer capacitor rated for 5 A pulses. Check the top of the range too: that cell’s 3.67 V open-circuit voltage is above the UWB transceiver’s 3.6 V maximum operating supply.
A lithium AA (lithium iron disulfide) cell is 1.5 V nominal with an internal resistance of about 0.1 to 0.2 ohms that barely changes between −20 °C and 40 °C, with depth of discharge or with age, against 10 ohms or more for a 2032. Two in series give about 3.0 V nominal, but a fresh cell’s open-circuit voltage is 1.79 to 1.83 V, so a fresh pair can reach 3.66 V, just above that 3.6 V maximum.
A rechargeable lithium-ion pouch cell is lower again: one 1,000 mAh cell’s sheet lists an impedance of 180 milliohms, without the test method, so take it as a scale. It charges to 4.2 V, above the transceiver’s maximum, so it needs a regulator as well as a charger, and typical cells mustn’t be charged below 0 °C (charge temperature limits).
A boost converter with the buffer capacitor on its input lets it swing further: if the converter runs down to 2.0 V (check its minimum input), ΔV on a mid-life cell widens from about 0.4 V to about 0.9 V, though it draws more charge as the voltage falls. One chip maker’s boost example cut its storage capacitor from 330 µF to 47 µF.
Measuring the sag on the bench
A bench supply has almost none of a coin cell’s internal resistance, so it hides the sag, and the test needs real cells, part-used, in the cold.
- Part-discharge the cells. Discharge at a modest constant current, logging the charge removed, to about half and to near the end of the rated capacity, using more than one vendor.
- Soak them cold. Chamber or freezer at the lowest operating temperature, thermocouple on the cell, until the cell gets there.
- Probe the cell and the pin. Measure at the cell and at the radio’s supply pin, DC-coupled with a short ground, triggered on the falling supply or a firmware-set pin, and capture the exchange and the refill.
- Read the trace. Compare the lowest voltage at the pin with the highest minimum supply on the rail. The step at a burst’s start is ESR, the slope is current over capacitance, the recovery is the refill.
- Measure the resistance. Divide the voltage step at the cell’s terminals by the current step, as the cell maker’s handbook does, with your pulse shape, at each depth and temperature. That gives you the table no maker publishes.
- Run the worst firmware case. Retries, the longest receive window, the highest transmit power, the higher UWB channel, and a BLE event landing on a UWB exchange.
Before I trust a coin-cell design, I want to see the radio’s supply pin on a scope during its heaviest burst, with a part-used cell in the cold; that one capture tells me more than any battery-life estimate built on averages.
If your tag has to range for months on a coin cell and you’d like the bursts, the capacitor and the cold case worked through against the datasheets, get in touch.