Articles

Do you need a battery protection circuit if the charger has limits?

Yes. A charger controls a normal charge, and it’s one of the things that can fail; a protection circuit (a protection IC and its switches, often called a PCM, or part of a BMS in a larger pack) is the independent layer that disconnects the cell when the charger, the load or the wiring has gone wrong. On a 4.2 V lithium-ion cell, pack protection boards typically stop charging at around 4.26 to 4.30 V, stop discharge at around 2.8 to 3.0 V, and cut overcurrent within milliseconds, or within 0.25 to 0.6 ms for a short circuit. The overcharge threshold sits just above the charger’s worst-case maximum, in a range a normal charge never reaches, and the margins on either side of it are tens of millivolts. Protection works with no firmware running, but it can’t stop an internal short in a damaged cell.

The terms used here (charge voltage, cutoff voltage, C-rate) are defined in How lithium-ion charging works. The charger’s own settings and tolerances have their own article; this one is about what protects the cell when the charger, the load or the wiring fails.

The layers, from the cell outward

Layer What it acts on Resets? Needs firmware?
Inside the cell: vent, current-interrupt device, PTC in some Gas pressure; heat in the PTC Vent and current-interrupt device: no No
Pack protection circuit and its two switches Overvoltage, undervoltage, charge and discharge overcurrent, short circuit Yes, once its release conditions are met No
Secondary overvoltage protection and three-terminal fuse Overvoltage that got past the primary No: the fuse is blown No
Series fuse Sustained overcurrent nothing else stopped No No
Thermistor and temperature cut-offs Cell too hot or too cold to charge or discharge Yes Depends where it’s read
The charger’s limits Charge voltage and current, temperature window, timers Yes Depends on the charger
The system’s limits Low-battery shutdown, load control Yes Usually

The charger and the system sit at the bottom on purpose: they’re the likeliest to be wrong, through a charger option set wrong, a firmware charger with bad calibration, or a product left on until the cell is flat. Protection assumes they’ve failed, which is why it’s built from comparators and switches with fixed delays. A processor that’s halted or running bad code can’t open a switch.

That also answers whether a charger’s own protections are enough. Many chargers have a battery overvoltage limit, a discharge cut-off and a battery switch of their own. They share the charger’s silicon, supply and reference, so a fault that takes out the charge control can take them out too: they’re useful, but they aren’t independent of the thing they’d be protecting against. A “protected cell” is one sold with a protection board already fitted, which covers this layer, with thresholds someone else chose.

I’ve written charge-control and protection firmware myself, for custom multi-cell packs. Firmware can add protection that sees trends and combinations a comparator can’t; it shouldn’t be the only protection.

Inside the cell

A teardown study of commercial 18650 cells found a current-interrupt device and a top vent in every cell it opened, and calls both mandatory for that format. The current-interrupt device is a pressure-operated disc that breaks the internal connection as gas builds, at about 1.0 to 1.2 MPa in that study; the vent opens at about 2.2 to 2.3 MPa. Both are one-shot. A PTC (positive temperature coefficient device, whose resistance rises sharply as it heats) is optional and left out of high-rate cells: one in the study, rated for 20 A continuous discharge, has none. For other cylindrical sizes, the datasheet or the maker has to say what’s inside. Pouch cells typically have neither a current-interrupt device nor a PTC; the heat-sealed edge acts as a vent, but nothing inside a pouch opens the circuit.

Nothing inside or outside the cell stops an internal short, which happens beyond the reach of any switch. The outer layers can avoid making one worse: the JEITA guideline on lithium-ion batteries in notebook computers notes that overcharging increases the possibility of an uncontrolled thermal state in case of an internal short, the best argument for an overvoltage limit that holds whatever the charger does.

The protection circuit and its two switches

On a single cell, the protection circuit is a small chip and two MOSFET switches in series with the cell, usually in the negative lead. The chip measures the cell voltage directly and the current as the voltage across the two switches. When a threshold stays crossed for longer than its delay, it turns a switch off. It runs from the cell, all the time, usually through a small resistor and capacitor on its supply pin, which hold it up while a short pulls the cell’s terminal voltage down; without them the chip can brown out at the moment it’s needed most.

Switching the negative lead has a side effect: once the protection opens, the system’s ground floats away from the cell’s negative. A thermistor line, a data line or a sense line that connects system and cell can then carry current the switch was meant to stop, or back-feed a part that should be off. Kelvin connections matter too: any trace resistance inside the current-sensing loop adds to the measured drop and lowers the trip current.

Why two, back to back

A MOSFET has a body diode built in from source to drain. Turned off, it blocks current one way only; the other way, current flows through the diode. So one switch can stop a discharge or a charge, never both. The protection uses two in series with their diodes pointing opposite ways. The usual single-cell arrangement joins their drains, with one source at the cell’s negative and the other at the pack’s, so the chip can drive each gate against its own source.

The discharge switch opens for undervoltage, discharge overcurrent and short circuit; its body diode still lets charge current in, so a charger can bring the cell back up. The charge switch opens for overvoltage and charge overcurrent; its body diode still lets the cell discharge, so the product can draw the cell back down. Release conditions vary by chip: one pack’s board releases an overvoltage trip at 4.18 ± 0.05 V, and one single-cell family releases an undervoltage trip once the cell has risen 100 mV above the trip and the voltage between the cell’s positive terminal and the pack’s negative terminal exceeds 1 V.

Current through an open switch’s body diode isn’t free. It drops a diode voltage, so the off switch heats by that voltage times the current, which matters if a charger keeps driving fast-charge current through it. And a charger looking at a pack whose discharge switch is open sees the cell plus a diode drop, so a deeply discharged cell can read high enough to skip precharge, and a zero-volt policy based on the voltage at the pack terminals isn’t reading the cell.

Current measured across the switches

Sensing across the switches saves a resistor and its loss, at the cost of accuracy. The chip’s thresholds are voltages (tabled below), so the trip current is the threshold divided by the on-resistance of the pair. With example switches of 5 mΩ each, 10 mΩ for the pair (the pairs read for single-cell protection run from about 4.5 to 18 mΩ typical at 4.5 V gate drive), and ignoring their unit-to-unit spread and the threshold’s own tolerance, a 100 mV threshold trips at 10 A and a 400 mV short-circuit threshold at 40 A.

On-resistance rises as the switches heat and falls with more gate drive, which in a single-cell pack comes from the cell, so it’s weakest when the cell is nearly flat. On the parts read, a gate at 3.8 V raises the resistance about 10 to 20 percent over the 4.5 V figure, 2.5 V raises it 30 to 80 percent, and at a 125 °C junction it’s about 1.4 to 1.5 times its 25 °C value. If the pair’s resistance rises by half, the same 100 mV trips at 6.7 A. The threshold has to clear the real peak current with the switches hot and the cell low, and still trip below what the wiring and cell can take with the switches cold and the cell full.

Setting the thresholds

Charger, cell and protection thresholds near 4.2 VFive bands on a voltage axis from 4.0 to 4.5 volts. The charger restarts charging when the cell falls to somewhere between 4.02 and 4.17 volts, once both tolerances are stacked. The charger holds between 4.16 and 4.23 volts, nominally 4.20. The cell's charge voltage is 4.20 volts plus or minus 0.05, so its limit is 4.25 volts. The protection circuit's overvoltage trip is 4.28 volts plus or minus 25 millivolts. A secondary overvoltage protector set at 4.35 volts trips between 4.30 and 4.40 volts.Recharge restarts below, both tolerances stacked4.02–4.17 VCharger’s held voltage, minimum to maximum4.16–4.23 VCell’s charge voltage, 4.20 V ± 0.05 Vmax 4.25 VProtection circuit overvoltage4.28 V ± 25 mVSecondary overvoltage (one option)4.35 V ± 50 mV4.0 V4.1 V4.2 V4.3 V4.4 V4.5 Vcell limit 4.25 V
Example thresholds near the top of charge for a 4.2 V cell, taken from the datasheets of one charger, one cell, one pack protection circuit and one secondary protector. The charger's held voltage can reach 4.23 V, 20 mV under the cell's 4.25 V limit, and the protection circuit trips only above that. Other parts give other numbers.
Product, protection and charger thresholds at the bottom of dischargeFive bands on a voltage axis from 1.5 to 3.6 volts, with the cell's 2.5 volt rated cutoff marked. From the top: the product's own low-battery shutdown, a design choice above the protection; pack protection undervoltage at 2.8 to 3.05 volts; the charger's precharge threshold, typically 2.5 to 3.0 volts; single-cell protection undervoltage options from 2.0 to 2.8 volts, plus or minus 50 millivolts; and the charger's battery-short threshold, 1.6 to 2.35 volts.Product’s own low-battery shutdown (a design choice)Pack protection undervoltage (two pack boards)2.8–3.05 VCharger precharge threshold (typical)2.5–3.0 VSingle-cell protection undervoltage options2.0–2.8 V ± 50 mVCharger battery-short threshold1.6–2.35 V1.5 V2.0 V2.5 V3.0 V3.5 Vcell’s rated cutoff 2.5 V
Example thresholds at the bottom of discharge for a 4.2 V lithium-ion cell, from several charger, protection and cell datasheets. The product should shut itself down first, above the protection circuit's undervoltage trip; the cell's rated cutoff, often 2.5 V, sits among the charger's precharge and battery-short thresholds. Protection options below the cell's cutoff suit other cells. The order matters more than the numbers, which differ between parts.

Overvoltage

Two limits get confused here. The charge-voltage limit is what the charger must stay under in normal charging: 4.25 V on a 4.20 V ± 0.05 V cell, and on one charger family that holds 4.23 V at most, 20 mV of margin. The overcharge-protection threshold is a fault limit, and it sits above that, in the range a normal charge should never reach (the JEITA guideline, describing secondary protection, calls it the overcharging range that should usually be inaccessible). A pouch cell sold with its own protection board trips at 4.26 to 4.30 V, 10 to 50 mV above 4.25 V, and a pack maker’s board at 4.28 V ± 25 mV, 5 to 55 mV above it. The tolerances article works the charger’s side corner by corner. One cell maker tells pack designers to set protection within the ranges in the cell specification; that’s the document to follow for a particular cell.

Cells whose datasheet states the charge voltage as an absolute maximum close the gap. A high-voltage pouch cell’s sheet says charging beyond 4.35 V per cell must be strictly prohibited, so the protection has to sit at or below 4.35 V, and the charger’s maximum below the protection’s lowest trip. With a 4.30 V option at ±20 mV, the trip can be as low as 4.28 V, so the charger’s maximum has to stay under that: a setting around 4.26 V at ±0.5 percent, and the capacity that costs is part of the design. The same sheet says it directly: “The charger and protection circuit of battery pack shall be designed to comply with this condition.”

The protection chip’s accuracy joins the budget: one single-cell family offers options from 3.85 to 4.60 V in 50 mV steps, ±10 mV at 25 °C and ±20 mV from 0 to 60 °C. So check that its lowest trip voltage, at tolerance and over temperature, sits above the charger’s highest held voltage. Where the bands overlap, some units disconnect at the top of every charge, which looks like a charger that stops early.

The overvoltage delay is long, 0.25 to 4.5 s on that family, about a second on the two boards and 1 to 8 s on a programmable pack monitor, so it doesn’t trip on noise or the steps of a pulsed charge current.

A wrong charger adds a voltage problem. When the charge switch opens, it holds off the charger’s voltage minus the cell’s, so the switch and the protection chip’s pins have to be rated for the highest-voltage charger that can physically be plugged in, or the protection fails short on the very fault it’s there for.

Undervoltage

At the bottom the order runs the other way. The product’s own low-battery shutdown comes first, so it turns off cleanly with some charge left for the months it may then sit. The protection’s undervoltage trip sits below it, as the backstop for a product that didn’t shut down or a load that stayed connected, and the cell’s rated cutoff, often 2.5 V, below both. The two boards read trip at 2.8 V and at 3.0 V ± 50 mV; a single-cell family offers 2.00 to 2.80 V, ±50 mV; a programmable monitor covers about 1.58 to 3.1 V. Options below the cell’s rated cutoff suit other cells; for this one, pick a trip above it. One cell maker warns that a leakage current to the equipment may over-discharge the cell.

A radio burst or a motor start can pull a part-charged cell’s terminal voltage under the threshold for a moment, by the current times the internal resistance. Undervoltage delays of 20 to 330 ms on the single-cell parts and boards read, and 1 to 16 s on the monitor, ride through that. The product’s shutdown needs the same care.

On one sample board, the firmware’s low-battery cutoff read the cell under heavy load, so the product shut down early. Reading at a quiet moment, or filtering across the load’s pulses, keeps the cutoff where it was meant to be.

Overcurrent, in tiers

Current protection is tiered, because the right delay depends on how far over the current is: a modest overload can be allowed for a while, a short has to be stopped at once. On the single-cell parts and boards read:

Fault Threshold (across the switches) Delay
Charge overcurrent 45 to 155 mV 4 to 16 ms
Discharge overcurrent 90 to 200 mV about 1 to 48 ms
Short circuit about 0.3 to 0.7 V 0.25 to 0.6 ms

A programmable pack monitor stretches the discharge tier to 8 to 1,280 ms and puts its short-circuit delay at 70 to 400 µs. The single-cell family’s delays carry ±20 percent tolerance.

The tiers let inrush ride through. Switching on into input capacitors, or starting a motor, draws a brief peak far above the running current, so the discharge threshold sits above the running current with a delay longer than the inrush, and the short-circuit threshold sits above the inrush peak. Charge overcurrent is there for the wrong charger: one set too high, or one built for a bigger pack.

After an overcurrent or short-circuit trip, the chip has to decide when to reconnect. Many wait until the load is removed, which they detect at the pack terminals; others retry. A product that retries into a standing short heats the switches on every attempt, so the release behaviour belongs in the design. And a fault current just under the lowest tier isn’t stopped by the protection at all: it flows for as long as the cell can supply it, and only a fuse or a thermal cut-off stands in its way.

Temperature

One cell sheet asks that a discharge over-temperature cut-off not be set above 60 °C cell surface temperature; a power cell recommends 80 °C at high rates. Both are surface temperatures, so the thermistor belongs on the cell, not next to a warm charger. Charge temperatures are in the temperature article.

Surviving a short

For those few hundred microseconds the switches carry whatever the short draws. As an example, not a bound: a cell with a DC resistance of 30 ± 6 mΩ, as one 21700 datasheet gives it, at 4.2 V, with the example 10 mΩ switch pair and an example 10 mΩ of wiring and contacts. At the cell’s low corner, 24 mΩ, the path totals 44 mΩ and the current is about 4.2 / 0.044 ≈ 95 A. Over a fraction of a millisecond the cell’s resistance is lower than that 30-second DC figure (the same sheet gives 25 mΩ or less at 1 kHz), and lower again when warm, so the real peak can be higher. The pair dissipates about 91 W, about 55 mJ over the slowest short-circuit delay read, 0.6 ms.

That figure is a floor, because it assumes the switches stay fully on. In the same example the cell’s terminals fall to about 4.2 − 95 × 0.024 ≈ 1.9 V, and the switches’ gate drive comes from the cell. If the gate voltage sags, the switches leave full enhancement and dissipate far more, and if the chip’s supply browns out, they may not turn off cleanly at all. That’s the usual way short-circuit protection fails, and why the supply filter and a check against the switches’ transient thermal ratings matter more than the energy number.

A short through a length of cable can be harder still. Its resistance can hold the current just under the short-circuit threshold, so it falls to the discharge tier: at the example 40 A, the pair dissipates 16 W for up to 48 ms, or 57.6 ms at the delay’s +20 percent tolerance, about 0.9 J. Energy alone isn’t the right comparison across such different pulse lengths; the switch’s transient thermal impedance curve is. Size the thresholds and switches for the worst short the wiring allows, not only one at the terminals.

Turning a large current off fast has its own problem: the wiring’s inductance drives the voltage across the opening switch up until something conducts, often the switch itself, in avalanche, and long leads make it worse. A switch rated for the avalanche energy, a clamp across the pack terminals or a slowed turn-off are the usual answers, settled by a measurement on the real wiring. In normal use the example pair drops 20 mV at 2 A, which moves the charger into constant voltage earlier, as the tolerances article works through.

Secondary protection and fuses

Primary protection resets, which is right after a short or a flat cell, and no help when its own charge switch has failed short while the charger keeps driving the cell up. Secondary overvoltage protection covers that: a separate comparator per cell, with its own reference and a fixed threshold above the primary’s. The families read offer 4.30 to 4.65 V, accurate to ±25 mV typical (±35 mV maximum) at 25 °C, ±50 mV from −20 to 85 °C and ±80 mV from −40 to 110 °C, with a delay set by a capacitor, 1 to 2 s with the datasheet’s example value. Its output typically fires a three-terminal fuse, a fuse with a heater element beside it that the protector drives until the fuse opens. Nothing resets that, and a blown fuse in the main current path stops discharge as well as charge.

The JEITA guideline is plain about what follows: “A battery where the above secondary protection has been triggered in the past must not be used. However, discharge shall be permitted.” A design that follows the second sentence latches off charging rather than blowing a fuse in the main path. The guideline also asks for the secondary threshold to be “as close to the upper limited charging voltage in each temperature range as possible”. That pulls it toward the primary, so check the two against each other at both edges. A secondary at 4.35 V ± 50 mV can trip at 4.30 V, overlapping the top of a 4.28 V ± 25 mV primary by 5 mV, and its delays overlap too, about 0.7 to 1.3 s on that primary against 1 to 2 s on the secondary, so on some units the fuse blows on an event the primary should have caught. At its top edge the same secondary doesn’t trip until 4.40 V, or 4.43 V over the wider temperature range, which has to be acceptable to the cell maker.

An ordinary fuse in series with the cell is the last layer for current, including current through a protection switch that has failed short. It needs a DC voltage rating at least the pack’s and a DC interrupting rating at least the cell’s short-circuit current at full charge; a DC arc has no zero crossing to put it out. Small surface-mount fuses for battery packs are rated, for example, to interrupt 50 A at 32 V DC, and fuse makers state that rating at their rated voltage with a battery source, so check it against the cell’s short-circuit current, not the pack’s running current: the example short above, about 95 A, is well past a 50 A rating. They also derate for continuous current (25 percent on two datasheets) and further for temperature. It also has to coordinate with the protection: survive the shorts the switches clear, and still open on a sustained fault. The example hard short, 95 A for 0.6 ms, is about 5.5 A²s, enough to blow or age a small fuse on an event the protection had already handled, so compare the fuse’s melting I²t with that and derate it for temperature. Put it close to the cell, so it protects the wiring too. A thermal cut-off bonded to the cell adds a layer for heat that no current threshold sees.

Single faults, as the safety standards see them

IEC 62368-1, the safety standard for audio, video, information and communication technology equipment up to 600 V, has an annex on equipment containing batteries and their protection circuits, with clauses on protection circuits and on charging safeguards for secondary lithium batteries, and the standard tests battery charging and discharging under single fault conditions. The idea is that with any one component failed, shorted or open, the remaining safeguards still keep the cell safe. A charger plus one protection circuit already survives any single fault on paper. Secondary protection is about two weaknesses in that argument: a latent fault, such as a protection switch that has failed short and goes unnoticed until the day the charger also fails, and a common cause, such as a wrong charger whose voltage destroys the charge switch at the moment it’s needed.

IEC 62133-2 covers cells and batteries under intended use and reasonably foreseeable misuse, with tests including external short circuit, overcharging, forced discharge and a forced internal short. A cell that passes it doesn’t make the product’s charging safe: the Canadian edition notes that it lacks specific requirements regarding charging. Which standards a product needs is covered in compliance by market.

After a trip: recovery, 0 V and the deadlock

An undervoltage trip leaves the cell disconnected near the trip voltage, and self-discharge and anything still connected keep pulling it down. One protection board quotes 4.0 µA typical and 8.7 µA maximum in operation, and 0.12 µA maximum in its static state, which a chip with a power-down mode enters after an undervoltage trip; a secondary protector, if fitted, quotes under 2 µA. The operating figure is the one that matters in storage before a trip: on a 150 mAh cell, 8.7 µA takes a full cell flat in about two years. Anything wired on the cell side of the protection switches, a sense divider, an ESD clamp, the secondary protector, keeps drawing after a trip, so the trip doesn’t stop it. One cell maker recommends charging a stored cell back to 30 percent if it approaches 2.5 V.

Then there’s the deadlock. After an undervoltage trip the discharge switch is open, the charge switch is still on, and the chip still runs from the cell, so charge current can reach the cell through the discharge switch’s body diode. Any charger that applies a voltage and a small current wakes it. The deadlock comes from chargers that wait to see a battery voltage at their output before they start: with the pack presenting little or nothing, the charger waits for the battery and the protection waits for the charger, and the product looks dead with a good cell inside. Chargers that apply a limited current when they see nothing break it (battery-short modes feed a few milliamps up to about 100 mA below roughly 1.6 to 2.35 V).

The protection chip’s zero-volt charging option is a different case: it decides whether a cell near 0 V, too low to power the chip and turn on the charge switch, may be charged at all, and one family allows it if the charger’s voltage is above 1.7 V. A part with zero-volt charging disabled still recovers from an ordinary undervoltage trip; it only refuses the cell that has gone all the way down. That’s usually the safer choice, because a cell driven toward 0 V can be damaged inside, as How lithium-ion charging works explains. Whatever the policy, the protection’s option, the charger’s short threshold and the firmware have to agree on it. Ship mode, where the product leaves the factory disconnected and wakes when a charger is plugged in, depends on the same handshake, so test it alongside.

Easy to miss on the board

  • A pouch cell with a protection board already fitted has thresholds chosen before your charger was: check them against the charger’s maximum and the product’s shutdown voltage. A bare one gets only the protection you add. -Reverse polarity. On one sample board, the cell connected through a hand-plugged connector with no reverse-polarity protection. Assume an unkeyed connector will go in backwards, and key it or add a reverse-polarity element that survives the cell’s short-circuit current. -No fuse. On another sample board, there was no fuse in series with the cell.
  • A ceramic capacitor straight across the cell. Capacitor makers warn that a flex crack can start open and become a short in the field, with heating or ignition when the supply has ample current, as a cell does. Keep it away from board edges, screws and connectors, and consider flexible-termination or open-mode parts: in one maker’s 10 mm bend test, every standard part cracked and no resin-electrode part did.
  • ESD on contacts a user can touch, which lands on the protection chip’s pins. Clamp it, and count the clamp’s leakage in the storage drain. -A sense divider left on the cell. On one sample board, a battery-sense divider drew about 20 µA with the product switched off, more than twice the worst protection drain above: on the same 150 mAh cell, about ten months from full to flat.
  • Hot-plugging into capacitance: a charged pack connected to a large input capacitance can trip its short-circuit tier on first connection and look dead. Large packs usually add a precharge circuit.

Series packs

In a series pack the cells drift apart, so the highest cell reaches its limit while the pack voltage still looks fine, and on discharge the weakest cell reaches undervoltage first. Run past that, the stronger cells can drive the weakest one below 0 V, into reversal, which is the condition that damages a cell inside. Protection has to measure every cell, and has to notice an open sense wire rather than read it as a healthy cell: secondary protectors for two to four cells compare each with its own reference, and pack monitors cover 3 to 15 cells. Current is usually measured across a sense resistor, which removes the switches’ temperature from the threshold but adds its own error: one monitor’s comparators have ±2.5 mV offset and ±10 percent scale accuracy, so across an example 2 mΩ resistor the offset alone is ±1.25 A. The switches have to hold off the pack voltage plus the spike from the wiring’s inductance at turn-off, and their heat sets how many there are and how they’re laid out. Balancing and the rest of a BMS are in their own article.

In large multi-cell packs, much of the protection work is in measuring every cell, measuring current accurately at both ends of its range, and getting the heat out of the switches.

Testing it

Test in an order where each step is safe even if the last one found a problem:

  1. No cell: power the charger input with nothing on the battery terminals, and check that nothing gets hot.
  2. A simulated cell, from a bench supply that can sink as well as source current. Sweep it through overvoltage and undervoltage, and measure each trip point, delay and release against the datasheet bands.
  3. Each current tier: an electronic load for discharge, a supply above the charge-overcurrent threshold, a switched short for the short-circuit tier, delays on a scope, switches cold and hot. Make the short with a low-inductance electronic switch, not a mechanical one that bounces.
  4. A tripped pack on every charger it might meet, and the zero-volt policy at the voltages it should accept and refuse.
  5. A real cell, attended, where a cell fire would be contained: a short at the pack terminals through the real wiring, with the cell full, cold and hot, repeated; the thermistor cut-off; a full charge and discharge; then sleep current with the product off.
  6. Single faults: short the charge switch and overcharge from a current-limited supply, and confirm the secondary protection or fuse acts.

Production test can’t trip every threshold on every unit, but it can confirm the protection is fitted and its switches open, with an overcurrent or short-circuit trip on the fixture and a check that the pack recovers (designing for production test).

If you’re setting protection thresholds for a cell, or checking a design where the charger, the protection and the firmware all have a say, get in touch.

All articles

Have a project in mind?

Based in southern Indiana. Working with clients anywhere, including companies across the Midwest.